Force measurements using Fe-rich amorphous wire as magnetostrictive delay line

Αποθετήριο DSpace/Manakin

Εμφάνιση απλής εγγραφής

dc.contributor.author Chiriac, H en
dc.contributor.author Hristoforou, E en
dc.contributor.author Neagu, M en
dc.contributor.author Borza, F en
dc.date.accessioned 2014-03-01T01:16:36Z
dc.date.available 2014-03-01T01:16:36Z
dc.date.issued 2001 en
dc.identifier.issn 0924-4247 en
dc.identifier.uri https://dspace.lib.ntua.gr/xmlui/handle/123456789/14105
dc.subject Amorphous positive magnetostrictive wires en
dc.subject Force sensors en
dc.subject Magnetoelastic effects en
dc.subject Magnetostrictive delay lines en
dc.subject.classification Engineering, Electrical & Electronic en
dc.subject.classification Instruments & Instrumentation en
dc.subject.other Annealing en
dc.subject.other Electric wire en
dc.subject.other Ferromagnetic materials en
dc.subject.other Force measurement en
dc.subject.other Iron compounds en
dc.subject.other Magnetic field effects en
dc.subject.other Magnetism en
dc.subject.other Sensors en
dc.subject.other Amorphous positive magnetostrictive wires en
dc.subject.other Amorphous wire en
dc.subject.other Force sensors en
dc.subject.other Magnetic annealing en
dc.subject.other Magnetoelastic effects en
dc.subject.other Magnetostrictive delay line en
dc.subject.other Amorphous materials en
dc.title Force measurements using Fe-rich amorphous wire as magnetostrictive delay line en
heal.type journalArticle en
heal.identifier.primary 10.1016/S0924-4247(01)00501-5 en
heal.identifier.secondary http://dx.doi.org/10.1016/S0924-4247(01)00501-5 en
heal.language English en
heal.publicationDate 2001 en
heal.abstract In this paper, we present experimental results concerning the heat treatment influence on the force response of Fe77.5Si7.5B15 amorphous wire used as magnetostrictive delay line (MDL). The amorphous wires, 125 mum diameter, were tested in the as-cast state, after stress-relief (thermally treated) and after magnetic annealing. The response of the delay line (pulsed output voltage) could be fitted by a linear curve at certain regions for the case of the as-cast amorphous wires and by an exponential curve for the case of treated wires. The sensitivity is equal to 10 mV/N, the minimum measurable change of the signal being 0.01 mV for the annealed wire corresponding to a minimum change of applied force equal to 0.001 N. (C) 2001 Elsevier Science B.V. All rights reserved. en
heal.publisher ELSEVIER SCIENCE SA en
heal.journalName Sensors and Actuators, A: Physical en
dc.identifier.doi 10.1016/S0924-4247(01)00501-5 en
dc.identifier.isi ISI:000168889000054 en
dc.identifier.volume 91 en
dc.identifier.issue 1-2 en
dc.identifier.spage 223 en
dc.identifier.epage 225 en


Αρχεία σε αυτό το τεκμήριο

Αρχεία Μέγεθος Μορφότυπο Προβολή

Δεν υπάρχουν αρχεία που σχετίζονται με αυτό το τεκμήριο.

Αυτό το τεκμήριο εμφανίζεται στην ακόλουθη συλλογή(ές)

Εμφάνιση απλής εγγραφής