HEAL DSpace

Interlaminar shear test for fibre-reinforced plastics

Αποθετήριο DSpace/Manakin

Εμφάνιση απλής εγγραφής

dc.contributor.author Sideridis, E en
dc.contributor.author Ashton, JN en
dc.contributor.author Kitching, R en
dc.date.accessioned 2014-03-01T01:41:50Z
dc.date.available 2014-03-01T01:41:50Z
dc.date.issued 1993 en
dc.identifier.issn 09544089 en
dc.identifier.uri https://dspace.lib.ntua.gr/xmlui/handle/123456789/23656
dc.relation.uri http://www.scopus.com/inward/record.url?eid=2-s2.0-0027147628&partnerID=40&md5=7e4d2636732019c9d868819205e572b9 en
dc.subject.other Crack propagation en
dc.subject.other Failure (mechanical) en
dc.subject.other Laminated composites en
dc.subject.other Mathematical models en
dc.subject.other Mechanical testing en
dc.subject.other Mechanical variables measurement en
dc.subject.other Photography en
dc.subject.other Shear strength en
dc.subject.other Four point bend method en
dc.subject.other Interlaminar shear strength en
dc.subject.other Interlaminar shear test en
dc.subject.other Glass fiber reinforced plastics en
dc.title Interlaminar shear test for fibre-reinforced plastics en
heal.type journalArticle en
heal.publicationDate 1993 en
heal.abstract The measurement of the interlaminar shear strength of glass-reinforced plastic (GRP) laminates is proposed using an offset four-point bend test on a beam where two (P) of the four forces differ from the other two (Q) and the ratio λ = P/Q depends upon the relative positions along the beam. The paper describes the development of this test which appears simpler, more economic and more realistic in many aspects than other test methods. It is demonstrated theoretically and experimentally that the span length (L), thickness (t) and the ratio λ are important test parameters in determining whether the failure is by shear or by flexure. A test rig was designed and constructed to investigate the influence of these parameters and to determine the interlaminar shear strength of a GRP laminate. Specimens were made from polyester resin containing E-glass fibres in the form of chopped strand mat (CSM). Clear and repeatable interlaminar shear failures have been obtained where L/t was relatively small and λ large. The crack formation mechanism was studied using photography. en
heal.journalName Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering en
dc.identifier.volume 207 en
dc.identifier.issue E1 en
dc.identifier.spage 61 en
dc.identifier.epage 72 en