Corrosion of yttria-fully stabilized zirconias in molten fluorides

Αποθετήριο DSpace/Manakin

Εμφάνιση απλής εγγραφής

dc.contributor.author Stournaras, C en
dc.contributor.author Tsetsekou, A en
dc.contributor.author Zambetakis, T en
dc.contributor.author Kontoyannis, C en
dc.contributor.author Carountzos, G en
dc.date.accessioned 2014-03-01T01:43:05Z
dc.date.available 2014-03-01T01:43:05Z
dc.date.issued 1995 en
dc.identifier.uri https://dspace.lib.ntua.gr/xmlui/handle/123456789/24036
dc.subject Crystal Structure en
dc.subject Grain Size en
dc.subject Microstructures en
dc.subject Phase Transformation en
dc.subject Raman Spectroscopy en
dc.subject X Ray Diffraction en
dc.title Corrosion of yttria-fully stabilized zirconias in molten fluorides en
heal.type journalArticle en
heal.identifier.primary 10.1007/BF00361520 en
heal.identifier.secondary http://dx.doi.org/10.1007/BF00361520 en
heal.publicationDate 1995 en
heal.abstract Yttria-fully stabilized zirconia ceramics were manufactured from home-made and commercially available powders and were sintered under different conditions. The ceramics were immersed in the corrosive environment of molten LiF, NaF, KF (FLINAK) eutectic for up to 360 h from 700–900 C. The changes caused in the crystal structure were probed with laser Raman spectroscopy and X-ray diffraction. The degree of en
heal.journalName Journal of Materials Science en
dc.identifier.doi 10.1007/BF00361520 en


Αρχεία σε αυτό το τεκμήριο

Αρχεία Μέγεθος Μορφότυπο Προβολή

Δεν υπάρχουν αρχεία που σχετίζονται με αυτό το τεκμήριο.

Αυτό το τεκμήριο εμφανίζεται στην ακόλουθη συλλογή(ές)

Εμφάνιση απλής εγγραφής