dc.contributor.author |
Gaki, A |
en |
dc.contributor.author |
Kakali, G |
en |
dc.contributor.author |
Wiglusz, RJ |
en |
dc.contributor.author |
Strek, W |
en |
dc.contributor.author |
Pasciak, G |
en |
dc.date.accessioned |
2014-03-01T02:47:05Z |
|
dc.date.available |
2014-03-01T02:47:05Z |
|
dc.date.issued |
2010 |
en |
dc.identifier.issn |
02555476 |
en |
dc.identifier.uri |
https://dspace.lib.ntua.gr/xmlui/handle/123456789/32991 |
|
dc.subject |
FTIR |
en |
dc.subject |
Impedance spectroscopy |
en |
dc.subject |
LSGM |
en |
dc.subject |
Polymeric precursor route |
en |
dc.subject |
Scanning electron microscopy (SEM) |
en |
dc.subject |
TG |
en |
dc.subject |
X-Ray diffraction (XRD) |
en |
dc.subject.other |
FTIR |
en |
dc.subject.other |
Impedance spectroscopy |
en |
dc.subject.other |
LSGM |
en |
dc.subject.other |
Polymeric precursor route |
en |
dc.subject.other |
SEM |
en |
dc.subject.other |
Calcination |
en |
dc.subject.other |
Diffraction |
en |
dc.subject.other |
Electric properties |
en |
dc.subject.other |
Fourier transform infrared spectroscopy |
en |
dc.subject.other |
Gallium |
en |
dc.subject.other |
Oxide minerals |
en |
dc.subject.other |
Perovskite |
en |
dc.subject.other |
Scanning electron microscopy |
en |
dc.subject.other |
Sintering |
en |
dc.subject.other |
Synthesis (chemical) |
en |
dc.subject.other |
X ray diffraction |
en |
dc.title |
Synthesis, characterization and electrical properties of single phase La0.9Sr0.1Ga0.8Mg0.2O3 |
en |
heal.type |
conferenceItem |
en |
heal.identifier.primary |
10.4028/www.scientific.net/MSF.636-637.874 |
en |
heal.identifier.secondary |
http://dx.doi.org/10.4028/www.scientific.net/MSF.636-637.874 |
en |
heal.publicationDate |
2010 |
en |
heal.abstract |
Single phase La0.9Sr0.1Ga0.8Mg 0.2O3-δ (LSGM9182) was synthesized by a polymeric precursor route. The XRD pattern after calcination at 1300 °C for 6h indicates the formation of the perovskite without the presence of secondary phases. XRD, FTIR and TG-DTG measurements were used to examine the powder precursor as well as the intermediate and final products. SEM images indicated the small grain size of the final product. The conductivity of the sintered sample was examined by means of a.c. impedance spectroscopy and was found to be 9 10-2 S/cm at 800 °C similar to the typical value of LSGM materials. © (2010) Trans Tech Publications. |
en |
heal.journalName |
Materials Science Forum |
en |
dc.identifier.doi |
10.4028/www.scientific.net/MSF.636-637.874 |
en |
dc.identifier.volume |
636-637 |
en |
dc.identifier.spage |
874 |
en |
dc.identifier.epage |
879 |
en |