HEAL DSpace

The size of plastic zones in cracked plates made of polycarbonate - The influence of the ratio of thickness to crack length on the size of plastic zones in polycarbonate plates was studied

Αποθετήριο DSpace/Manakin

Εμφάνιση απλής εγγραφής

dc.contributor.author Theocaris, PS en
dc.contributor.author Gdoutos, EE en
dc.date.accessioned 2014-03-01T01:05:34Z
dc.date.available 2014-03-01T01:05:34Z
dc.date.issued 1975 en
dc.identifier.issn 00144851 en
dc.identifier.uri https://dspace.lib.ntua.gr/xmlui/handle/123456789/8879
dc.subject bisphenol a en
dc.subject Three Dimensional en
dc.subject Yield Stress en
dc.subject.other POLYCARBONATES en
dc.title The size of plastic zones in cracked plates made of polycarbonate - The influence of the ratio of thickness to crack length on the size of plastic zones in polycarbonate plates was studied en
heal.type journalArticle en
heal.identifier.primary 10.1007/BF02319142 en
heal.identifier.secondary http://dx.doi.org/10.1007/BF02319142 en
heal.publicationDate 1975 en
heal.abstract The influence of the thickness of a cracked plate, made of Polycarbonate of Bisphenol A, on the plastic zones developed at the crack tip was studied. The three-dimensional character of yielding at the vicinity of the crack tip is revealed. The study of the thickness variation in the plastic zones is made by applying the shadow-moiré method. It has been derived that the thickness variation in the plastic zones is discontinuous with successive dimples of different thickness. The influence of the overall thickness of the specimen on the size and length of the plastic zone was studied for different crack lengths. Irwin's theory for small yielding, as well as the simple and modified Dugdale-Barenblatt models, were applied for the study of plastic zones. By comparing the plastic-zone lengths in relation to their shape, with those given by the above theories, it may be concluded that, for small loads where the applied stress σ is not exceeding 0.40 of the yield stress {Mathematical expression} in tension and small values of the ratio of crack length a to plate thickness t, (a/t<4) a state of plane strain dominates at the vicinity of the crack tip, while, by increasing the load and ratio a/t, the plastic zones approach in shape and size those given by the modified Dugdale-Barenblatt model. © 1975 Society for Experimental Mechanics, Inc. en
heal.publisher Kluwer Academic Publishers en
heal.journalName Experimental Mechanics en
dc.identifier.doi 10.1007/BF02319142 en
dc.identifier.volume 15 en
dc.identifier.issue 5 en
dc.identifier.spage 169 en
dc.identifier.epage 176 en


Αρχεία σε αυτό το τεκμήριο