dc.contributor.author |
Papaspyrides, CD |
en |
dc.contributor.author |
Diakoulaki, DC |
en |
dc.date.accessioned |
2014-03-01T01:06:39Z |
|
dc.date.available |
2014-03-01T01:06:39Z |
|
dc.date.issued |
1986 |
en |
dc.identifier.issn |
01937197 |
en |
dc.identifier.uri |
https://dspace.lib.ntua.gr/xmlui/handle/123456789/9539 |
|
dc.subject |
Poly Vinyl Chloride |
en |
dc.subject.other |
PIPE, PLASTIC - Recycling |
en |
dc.subject.other |
PLASTICS - Mechanical Properties |
en |
dc.subject.other |
WASTE UTILIZATION |
en |
dc.subject.other |
WATER - Applications |
en |
dc.subject.other |
MECHANICAL PROPERTIES RETENTION |
en |
dc.subject.other |
PLASTICS WASTE |
en |
dc.subject.other |
REUSABLE POLY(VINYL CHLORIDE) RECOVERY |
en |
dc.subject.other |
POLYVINYL CHLORIDE |
en |
dc.title |
RECOVERY OF REUSABLE POLY(VINYL CHLORIDE) FROM PLASTICS WASTE. |
en |
heal.type |
journalArticle |
en |
heal.identifier.primary |
10.1002/vnl.730080211 |
en |
heal.identifier.secondary |
http://dx.doi.org/10.1002/vnl.730080211 |
en |
heal.publicationDate |
1986 |
en |
heal.abstract |
Solvent recycling of poly(vinyl chloride) (PVC), on the basis of the cyclohexanone/n-hexane system, is studied. By using water during the washing stage, hexane quantities employed and solvents separation costs involved are drastically reduced. The modification proposed does not result in any alteration of the main characteristics of the process which further can be extended to rigid PVC pipes. No degradation effects were detected while the polymer recycled exhibits mechanical properties comparable with those of the virgin grade PVC especially with waste material of low additives content. Nevertheless, even from pipes, the polymer recovered proved quite suitable for similar applications. |
en |
heal.journalName |
Journal of Vinyl and Additive Technology |
en |
dc.identifier.doi |
10.1002/vnl.730080211 |
en |
dc.identifier.volume |
8 |
en |
dc.identifier.issue |
2 |
en |
dc.identifier.spage |
83 |
en |
dc.identifier.epage |
85 |
en |