dc.contributor.author |
Ammus Jamal, M |
en |
dc.contributor.author |
Androutsopoulos George, P |
en |
dc.contributor.author |
Tsetsekou Athena, H |
en |
dc.date.accessioned |
2014-03-01T01:06:44Z |
|
dc.date.available |
2014-03-01T01:06:44Z |
|
dc.date.issued |
1987 |
en |
dc.identifier.issn |
0888-5885 |
en |
dc.identifier.uri |
https://dspace.lib.ntua.gr/xmlui/handle/123456789/9600 |
|
dc.relation.uri |
http://www.scopus.com/inward/record.url?eid=2-s2.0-0023382353&partnerID=40&md5=278886b77b7447f8a273dd672d722007 |
en |
dc.subject.classification |
Engineering, Chemical |
en |
dc.subject.other |
CATALYSIS |
en |
dc.subject.other |
CHEMICAL EQUIPMENT - Reactors |
en |
dc.subject.other |
CHEMICAL REACTIONS - Desulfurization |
en |
dc.subject.other |
COKE DEPOSIT |
en |
dc.subject.other |
GREEK OIL RESIDUE |
en |
dc.subject.other |
HDS CATALYSTS |
en |
dc.subject.other |
HYDRODESULFURIZATION |
en |
dc.subject.other |
PORE STRUCTURE |
en |
dc.subject.other |
CATALYSTS |
en |
dc.title |
INVESTIGATION OF THE DEACTIVATION PHENOMENA ASSOCIATED WITH THE USE OF COMMERCIAL HDS CATALYSTS. |
en |
heal.type |
journalArticle |
en |
heal.language |
English |
en |
heal.publicationDate |
1987 |
en |
heal.abstract |
Catalyst deactivation data, obtained from the HDS of a Greek oil residue on a spinning basket laboratory scale reactor, are reported in this paper. Two commercial grade hydrodesulfurization (HDS) catalysts, viz. , Harshaw HT-400 E and ICI-41-6, were used in the investigation. Initial activities and modes of activity loss vs. run time are compared (HT-400 E possessed an initial activity 25% higher than that of ICI-41-6; activity was reduced to 55-65% for the former and 70% for the latter catalyst after 100 h of operation). Coke and metal deposits built up vs. run time are also reported. It is shown that C/H ratios and N//2 content of coke deposits increased proportionally with operating time. Pore volume and surface areas (% of initial value after 30 h of operation) respectively reduced for HT-400 E to 43-57 and 40-45 and for ICI-41-6 to 60-70 and 40-45. Pore structure recovery parameters following reactivation ranged between 80% and 95% of their respective initial values. |
en |
heal.publisher |
AMER CHEMICAL SOC |
en |
heal.journalName |
Industrial and Engineering Chemistry Research |
en |
dc.identifier.isi |
ISI:A1987J176500009 |
en |
dc.identifier.volume |
26 |
en |
dc.identifier.issue |
7 |
en |
dc.identifier.spage |
1312 |
en |
dc.identifier.epage |
1323 |
en |